# Wear Parts, Bushings & Pins for Agricultural Machinery – Application Case

> Typical components for agricultural machinery: pins in 42CrMo4 QT, bimetallic bushings, wear parts and quick couplings. Batches 2,000–20,000 pcs with cost-focused series supply.

https://www.sinbo-machining.com/case/agricultural-wear-parts/

---

## On This Page

  - Typical component families
  - Typical supply parameters
- Parameter Quick Reference
- Industry scenario: down-cycle cost pressure opens sourcing windows
- Typical component families and processes
- Workflow: drawing, sample approval and recurring series
- Quality and documentation
- FAQ
  - Related Materials · Related Services · Related Case Studies
- Planning components like these?

# Wear Parts, Bushings & Pins for Agricultural Machinery
Typical components for agricultural machinery: pins in 42CrMo4 QT, bimetallic bushings, wear parts and quick couplings. Batches 2,000–20,000 pcs with cost-focused series supply. Application at a glance
### Typical component families

|  Pins |  42CrMo4 QT, forged/turned + ground
|  Bushings |  Bimetallic steel + copper alloy
|  Quick couplings |  Steel, brass, Swiss-turned

### Typical supply parameters

|  Batch range |  2,000–20,000 pcs per family
|  Tolerance scheme |  DIN ISO 2768-mK, drawing fits
|  Documentation |  EN 10204 3.1, heat-treatment records

## Parameter Quick Reference

|  Parameter |  Specification
|  Component families |  Bolzen (pins); Buchsen (bushings); Verschleißteile (wear parts); Gelenkwellen-Komponenten (joint shaft components)
|  Typical materials |  42CrMo4 (quenched & tempered); bimetallic steel + copper alloy; wear-resistant steel + heat treatment; C45, 42CrMo4
|  Machining processes |  cold forging or turning + grinding; turning; turn-milling + coordinated HT; Swiss-type turning
|  Typical batch sizes |  2,000–20,000 pcs per family
|  Default tolerance scheme |  DIN ISO 2768-mK, drawing fits
|  Material certificates |  EN 10204 3.1, heat-treatment records
|  Inspection requirement |  first article inspection
|  Quotation and sample lead time |  quotation within 48 hours; first samples in 7–15 days

## Industry scenario: down-cycle cost pressure opens sourcing windows
Agricultural machinery procurement swings with the harvest cycle. In down years, cost-down programs push OEMs to re-source wear and linkage components — pins, bushings, wear plates — from competitive suppliers, while quality requirements (hardened pins, bimetallic bushings) stay unchanged. The component families are standardized across the industry: quenched-and-tempered pins, bimetallic bushings, wear parts with heat treatment, and quick couplings — in batches from 2,000 to 20,000 pieces with recurring demand.
## Typical component families and processes

|  Component (DE / EN) |  Typical material |  Process |  Typical batch
|  Bolzen (pins) |  42CrMo4 (quenched & tempered) |  cold forging or turning + grinding |  2,000–20,000 pcs
|  Buchsen (bushings) |  bimetallic steel + copper alloy |  turning |  2,000–20,000 pcs
|  Verschleißteile (wear parts) |  wear-resistant steel + heat treatment |  turn-milling + coordinated HT |  500–5,000 pcs
|  Gelenkwellen-Komponenten (joint shaft components) |  C45, 42CrMo4 |  turning |  500–5,000 pcs
|  Schnellkupplungen (quick couplings) |  steel, brass |  Swiss-type turning |  2,000–20,000 pcs
Heat treatment is coordinated as part of the process chain; hardness and case depth are confirmed per drawing.
## Workflow: drawing, sample approval and recurring series
The standard flow: drawing review and quotation within 48 hours, first samples in 7–15 days, first article inspection and approval, then series production against the approved reference. Batch sizes follow the table above — from single spare parts to tens of thousands of pieces per order, depending on the component family. For repeat orders, tooling, program revisions and inspection records are kept on file, so call-offs remain consistent with the approved first article. Engineering changes — material substitutions, tolerance updates, packaging changes — are handled as controlled changes against the same records.
## Quality and documentation
DIN ISO 2768-mK applies as the default tolerance scheme for unspecified dimensions. EN 10204 3.1 inspection certificates are standard for metallic parts, First Article Inspection supports the approval step, and RoHS/REACH declarations are available where required. Surface treatment, cleanliness and packaging requirements are confirmed per drawing.
## FAQ
Can you supply quenched-and-tempered pins?Yes — 42CrMo4 pins with QT condition, ground after heat treatment where the drawing requires it, with treatment records. How do bimetallic bushings work?Bimetallic strips (steel backing + copper alloy lining) are turned to size; the lining provides the bearing surface. What makes agricultural sourcing different?Down-cycle cost pressure — pricing decides, but hardened-pin quality and documentation expectations stay the same as in automotive-adjacent supply. Which batch sizes are typical?2,000–20,000 pieces per family for pins and bushings; wear parts from 500 pieces.
### Related Materials · Related Services · Related Case Studies
[Related Materials: Steel ](https://www.sinbo-machining.com/products/materials/steel/)[Related Services: Cold Heading ](https://www.sinbo-machining.com/services/cold-heading/)[Related Case Studies: Au Agricultural Machinery ](https://www.sinbo-machining.com/case/au-agricultural-machinery/)[· Ca Agri Equipment ](https://www.sinbo-machining.com/case/ca-agri-equipment/)This page describes a representative application scenario for the agricultural machinery manufacturing industry, compiled from typical requirements of this vertical. It is not tied to any specific customer or order; series quantities, materials and tolerances are confirmed per drawing for each enquiry.
## Planning components like these?
Send your drawing — Sinbo Precision will review material, tolerance scheme and batch plan and return a quotation within 48 hours. Samples in 7–15 days. [Get a Quote in 48 Hours ](https://www.sinbo-machining.com/quote/)