# Eyewear Hinge Components: Cold Forging + CNC Turning – Application Case

> Typical eyewear hinge components: hinge bodies, screws Ø1.0–1.8 mm, hinge pins and cold-forged blanks in brass and stainless. Swiss turning + cold forging, series from 10,000 pcs, RoHS/REACH.

https://www.sinbo-machining.com/case/eyeglass-hinges/

---

## On This Page

  - Typical component families
  - Typical supply parameters
- Parameter Quick Reference
- Industry scenario: hinge components are the outsourced core
- Typical component families and processes
- Workflow: drawing, sample approval and recurring series
- Quality and documentation
- FAQ
  - Related Materials · Related Services · Related Case Studies
- Planning components like these?

# Eyewear Hinge Components: Cold Forging + CNC Turning
Typical component families for eyewear manufacturing — hinge bodies, eyewear screws, hinge pins and cold-forged blanks in brass and stainless — with the cold forging plus CNC turning combination this category runs on. Application at a glance
### Typical component families

|  Hinge bodies / box |  Brass CuZn39Pb3, stainless
|  Eyewear screws Ø1.0–1.8 |  Stainless, nickel-plated brass
|  Cold-forged blanks |  Brass, steel, forged 60–180 T

### Typical supply parameters

|  Batch range |  10,000–50,000+ pcs per family
|  Tolerance scheme |  ±0.005 mm on guide diameters
|  Documentation |  EN 10204 3.1, RoHS/REACH

## Parameter Quick Reference

|  Parameter |  Specification
|  Component families |  corpi cerniera / box (hinge bodies); viti occhialeria Ø1.0–1.8 (eyewear screws); perni / pernolini (hinge pins); semilavorati a freddo (cold-forged blanks)
|  Typical materials |  CuZn39Pb3 brass, stainless; stainless, nickel-plated brass; 303 stainless, brass; brass, steel
|  Machining processes |  Swiss-type turning; Swiss turning + thread rolling; Swiss turning + grinding; cold forging (60–180 T)
|  Typical batch sizes |  10,000–50,000+ pcs per family
|  Default tolerance scheme |  ±0.005 mm on guide diameters
|  Material certificates |  EN 10204 3.1, RoHS/REACH
|  Inspection requirement |  first article inspection
|  Quotation and sample lead time |  quotation within 48 hours; first samples in 7–15 days

## Industry scenario: hinge components are the outsourced core
Eyewear manufacturers concentrate on design, brands and final assembly; the hinge — bodies, screws, pins and the cold-forged blanks they start from — is almost universally outsourced. The category runs on a two-process combination: cold forging for the near-net blanks and CNC Swiss turning for the finished precision features. Component families are variant-rich (screw lengths, pin diameters, body styles per collection) and demand tight guide-diameter tolerances, 100% thread checks and plating-ready surfaces — with collections refreshing every season, stable repeat supply matters as much as the first approval.
## Typical component families and processes

|  Component |  Typical material |  Process |  Typical batch
|  corpi cerniera / box (hinge bodies) |  CuZn39Pb3 brass, stainless |  Swiss-type turning |  ≥10,000 pcs
|  viti occhialeria Ø1.0–1.8 (eyewear screws) |  stainless, nickel-plated brass |  Swiss turning + thread rolling |  ≥50,000 pcs
|  perni / pernolini (hinge pins) |  303 stainless, brass |  Swiss turning + grinding |  ≥10,000 pcs
|  semilavorati a freddo (cold-forged blanks) |  brass, steel |  cold forging (60–180 T) |  ≥30,000 pcs
Guide diameters are held to ±0.005 mm, threads are checked 100%, and plating (nickel or nickel-free on request) plus aesthetic finishes are confirmed on samples per collection.
## Workflow: drawing, sample approval and recurring series
The standard flow: drawing review and quotation within 48 hours, first samples in 7–15 days, first article inspection and approval, then series production against the approved reference. Tooling, program revisions and inspection records are kept on file so that call-offs remain consistent with the approved first article. Engineering changes — material substitutions, tolerance updates, plating or packaging changes — are handled as controlled changes against the same records.
## Quality and documentation
DIN ISO 2768-mK applies as the default tolerance scheme for unspecified dimensions. EN 10204 3.1 inspection certificates are standard for metallic parts, First Article Inspection supports the approval step, and RoHS/REACH declarations are available where required. Plating, cleanliness and packaging requirements are confirmed per drawing.
## FAQ
Can you develop hinges from a technical drawing?Yes — from 2D/3D drawing to approved sample, with a dimensional report on every guide feature. What are the economic minimums?Swiss-turned parts from 10,000 pieces; cold-forged blanks from 30,000 pieces. Both routes can be quoted side by side for comparison. Which finishes can you prepare for?Nickel plating (nickel-free on request) and dark finishes via partners; aesthetic surfaces (mirror/satin) are confirmed on samples. Which documents accompany the parts?EN 10204 3.1 certificates and RoHS/REACH declarations as standard; dimensional reports per batch.
### Related Materials · Related Services · Related Case Studies
[Related Materials: Copper ](https://www.sinbo-machining.com/products/materials/copper/)[Related Services: Cold Heading ](https://www.sinbo-machining.com/services/cold-heading/)[Related Case Studies: Cosmetics Blanks ](https://www.sinbo-machining.com/case/cosmetics-blanks/)[· Special Fasteners ](https://www.sinbo-machining.com/case/special-fasteners/)This page describes a representative application scenario for the eyewear manufacturing industry, compiled from typical requirements of this vertical. It is not tied to any specific customer or order; series quantities, materials and tolerances are confirmed per drawing for each enquiry.