# Ti-6Al-4V Beta C Titanium Parts | Beta Alloy

> Ti-6Al-4V Beta C titanium alloy parts for defense and aerospace applications. Ultra-high strength beta titanium with excellent fracture toughness and ballistic protection.

https://www.sinbo-machining.com/products/materials/titanium/ti-6al-4v-beta-c-titanium/

---

## On This Page

- Quick Specifications
- Product Overview
- Key Features & Advantages
  - Ultra-High Strength
  - Fracture Toughness
  - Ballistic Protection
  - Lightweight
  - High Temperature
  - ITAR Compliant
- Technical Specifications
- Defense & Aerospace Applications
  - Missile Airframes
  - Armor Plating
  - Aircraft Structures
  - ordnance
  - Satellite Components
  - Personal Protection
- Frequently Asked Questions
  - What is Ti-6Al-4V Beta C?
  - What makes Beta C different from standard Ti-6Al-4V?
  - What is the ballistic rating of Beta C titanium?
  - Is Beta C titanium ITAR controlled?
- Related Products
  - Grade 5 Titanium Components
  - Grade 2 Titanium CNC Parts
  - Custom Titanium Machining
  - Aerospace Titanium Parts
- Ready to Get Started?

[Ti-6Al-4V Beta C Titanium Parts - Beta Titanium Alloy Components]  [Beta Titanium Component]  [Titanium Armor Plating]  [Missile Airframe Component]  [Ballistic Protection Titanium]
# Ti-6Al-4V Beta C Titanium Parts

## Quick Specifications
Material Ti-6Al-4V Beta C Process CNC Machining, Heat Treatment Tensile Strength 1170 MPa Lead Time 14-21 days MOQ 10 pieces Ballistic Rating Level III [Get Instant Quote ](https://www.sinbo-machining.com/quote?product=ti-6al-4v-beta-c-titanium)[Contact Us ](https://www.sinbo-machining.com/contact/)
## Product Overview
Ti-6Al-4V Beta C is a beta-rich titanium alloy specifically designed for applications requiring ultra-high strength, excellent fracture toughness, and ballistic protection. This advanced alloy offers superior mechanical properties compared to standard Ti-6Al-4V, making it ideal for critical defense and aerospace applications including missile airframes, armor plating, and high-performance structural components. Our Ti-6Al-4V Beta C components are manufactured using precision CNC machining and specialized heat treatment processes to achieve optimal beta phase distribution and mechanical properties. The alloy's unique chemistry and processing provide exceptional combination of strength (1170 MPa tensile), toughness (77 MPa√m fracture toughness), and ballistic performance (NIJ Level III). We specialize in producing mission-critical titanium components for defense contractors, aerospace manufacturers, and specialty applications requiring the highest levels of performance and reliability. Our expertise in beta titanium alloys ensures consistent quality and compliance with stringent defense and aerospace specifications.
## Key Features & Advantages

### Ultra-High Strength
Tensile strength of 1170 MPa for demanding applications
### Fracture Toughness
Excellent toughness of 77 MPa√m for damage tolerance
### Ballistic Protection
NIJ Level III ballistic resistance for armor plating
### Lightweight
Density of 4.65 g/cm³ for weight reduction vs steel
### High Temperature
Service temperature up to 300°C (572°F)
### ITAR Compliant
ITAR registered for defense applications
## Technical Specifications

|  Material |  Ti-6Al-4V Beta C Titanium Alloy
|  Condition |  Solution Treated and Aged (STA)
|  Tensile Strength |  1170 MPa (170 ksi)
|  Yield Strength |  1100 MPa (160 ksi)
|  Elongation |  10% in 4D
|  Fracture Toughness |  77 MPa√m (70 ksi√in)
|  Density |  4.65 g/cm³
|  Ballistic Rating |  NIJ Level III / STANAG 4569 Level 3
|  Surface Finish |  Anodized, Polished, CNC machined
|  Lead Time |  14-21 days depending on complexity
|  MOQ |  10 pieces for standard parts, negotiable for custom

## Defense & Aerospace Applications

### Missile Airframes
Structural components for missile and rocket systems
### Armor Plating
Ballistic protection panels and vehicle armor
### Aircraft Structures
High-stress airframe components and fasteners
### ordnance
Artillery shell casings and projectile components
### Satellite Components
Spacecraft structural parts and mechanisms
### Personal Protection
Body armor plates and protective equipment
## Frequently Asked Questions

### What is Ti-6Al-4V Beta C?
Ti-6Al-4V Beta C is a beta-rich modification of the standard Ti-6Al-4V alloy, specifically designed to increase beta phase stability and improve fracture toughness. It provides ultra-high strength (1170 MPa tensile) combined with excellent damage tolerance, making it ideal for ballistic and armor applications.
### What makes Beta C different from standard Ti-6Al-4V?
Beta C contains higher beta stabilizers (vanadium) which increases the volume fraction of beta phase after heat treatment. This results in significantly higher fracture toughness (77 MPa√m vs 44 MPa√m for standard Ti-6Al-4V) and better ballistic performance, while maintaining comparable strength.
### What is the ballistic rating of Beta C titanium?
Ti-6Al-4V Beta C meets NIJ Level III ballistic standards and STANAG 4569 Level 3 requirements, providing effective protection against handgun and rifle threats. Its combination of low weight and ballistic performance makes it superior to steel armor for many applications.
### Is Beta C titanium ITAR controlled?
Yes, as a high-performance titanium alloy used in defense applications, Ti-6Al-4V Beta C is subject to ITAR (International Traffic in Arms Regulations) controls. We are ITAR registered and compliant with all export control requirements for defense-related manufacturing.
## Related Products
 [Grade 5 Titanium Components]
### Grade 5 Titanium Components
Ti-6Al-4V titanium alloy [Learn More → ](grade-5-titanium-components) [Grade 2 Titanium CNC Parts]
### Grade 2 Titanium CNC Parts
Commercially pure titanium [Learn More → ](grade-2-titanium-cnc-parts) [Custom Titanium Machining]
### Custom Titanium Machining
Precision titanium services [Learn More → ](custom-titanium-machining) [Aerospace Titanium Parts]
### Aerospace Titanium Parts
AS9100 certified titanium [Learn More → ](aerospace-titanium-parts)