# Surface Finishing Services | CNC Parts Finishing

> Surface finishing for CNC parts: anodizing, plating, powder coating, polishing and more to improve durability, corrosion resistance and appearance.

https://www.sinbo-machining.com/services/finishing-services/

---

## On This Page

- Professional Surface Finishing Solutions
  - Why Choose Our Finishing Services?
- Surface Finishing Processes
  - Anodizing
  - Plating
  - Powder Coating
  - Polishing
  - Bead Blasting
  - Electropolishing
- Technical Specifications
  - Equipment Capabilities
  - Quality Standards
- Industries We Serve
  - Automotive
  - Medical
  - Electronics
  - Aerospace
- Frequently Asked Questions
- Start Your Finishing Project Today

# Finishing Services
20+ Finishing Methods 1000×1000mm Part Size Advanced Equipment ISO 9001 Certified
## Professional Surface Finishing Solutions
Surface finishing is a critical stage in the manufacturing process that significantly enhances product appearance, corrosion resistance, wear resistance, and functionality. Our comprehensive finishing services cover various post-processing needs for metal and plastic parts. From simple deburring and polishing to complex anodizing and plating treatments, we have advanced equipment and experienced technical teams to ensure every part meets expected surface quality requirements.
### Why Choose Our Finishing Services?
- Wide range of finishing processes and materials
- ISO 9001:2015 certified quality system
- Fast turnaround time: 3-7 days
- Expert team with 15+ years experience
 [Surface Finishing Workshop]
## Surface Finishing Processes
Comprehensive surface treatment solutions for various materials and applications
### Anodizing
Electrochemical process that creates a protective oxide layer on aluminum and other metals, enhancing corrosion resistance and enabling color dyeing. Thickness: 5-25μm Colors: Various Materials: Aluminum, Ti, Mg
### Plating
Metal coating process that deposits a thin layer of metal onto the surface, providing enhanced corrosion resistance, conductivity, and aesthetic appeal. Types: Zn, Ni, Cr, Au, Ag Thickness: 2-50μm Materials: Most Metals
### Powder Coating
Dry finishing process that applies a free-flowing dry powder electrostatically and cures under heat, creating a hard, durable finish. Thickness: 50-150μm Colors: Unlimited Materials: Metal, Plastic
### Polishing
Abrasive process that smooths and shines surfaces to achieve mirror-like finishes, removing scratches and imperfections for enhanced aesthetics. Roughness: Ra 0.1-0.8μm Finish: Mirror Materials: All Metals
### Bead Blasting
Surface treatment that propels abrasive media at high velocity to clean, smooth, or texture surfaces, creating uniform matte finishes. Media: Glass, Alumina, Steel Finish: Matte Materials: All Metals
### Electropolishing
Electrochemical process that removes material from the surface, improving micro-finish, reducing surface roughness, and enhancing corrosion resistance. Roughness: Ra 0.2-0.8μm Removal: 10-50μm Materials: Stainless Steel
## Technical Specifications
Detailed capabilities and quality standards
### Equipment Capabilities
Part Size 1000×1000mm Coating Thickness 5-150μm Temperature Control ±2°C Surface Roughness Ra 0.1-3.2μm Processing Capacity 5000+ parts/day
### Quality Standards

#### ISO 9001:2015
Quality management system certification
#### Salt Spray Testing
Corrosion resistance verification
#### Thickness Measurement
Coating thickness verification
#### Visual Inspection
Surface quality assessment
## Industries We Serve
Trusted by leading companies across various industries
### Automotive
Engine components, chassis parts, decorative finishes
### Medical
Surgical instruments, implants, medical devices
### Electronics
Connectors, housings, heat sinks
### Aerospace
Aircraft components, fasteners, structural parts
## Frequently Asked Questions
Common questions about our finishing services We offer a comprehensive range of surface finishing processes including anodizing, plating (zinc, nickel, chrome, gold, silver), powder coating, polishing, bead blasting, and electropolishing. Each process is tailored to meet specific material requirements and application needs. Our standard turnaround time is 3-7 days depending on the process, quantity, and complexity of the parts. Rush services are available for urgent projects with expedited processing options. We can finish a wide range of materials including aluminum, stainless steel, carbon steel, titanium, magnesium, copper, brass, and various plastics. Each material has specific finishing requirements and compatible processes. Yes, we are ISO 9001:2015 certified and provide quality documentation including material certificates, inspection reports, and test results upon request. We also conduct salt spray testing and other quality verification procedures.
## Start Your Finishing Project Today
Get in touch with our experts for professional consultation and competitive quotes [Get Quote ](https://www.sinbo-machining.com/quote/)[Consult Expert ](https://www.sinbo-machining.com/contact/)