# Powder Metallurgy: Materials, Density, Tolerances

> Powder metallurgy manufacturing for high-volume metal parts, covering material options, density targets, pressing, sintering, tolerances and secondary finishing.

https://www.sinbo-machining.com/services/powder-metallurgy/

---

## On This Page

- Precision Powder Metallurgy
- Powder Metallurgy Process
  - Powder Mixing
  - Compaction
  - Sintering
  - Finishing
- Technical Capabilities
  - Equipment Specifications
  - Material Systems
  - Quality Standards
- Industry Applications
  - Automotive
  - Industrial Machinery
  - Consumer Goods
- Ready to Start Your Powder Metallurgy Project?
- Start Your Manufacturing Project Today

[Home ](https://www.sinbo-machining.com/)[Services ](https://www.sinbo-machining.com/services/)[Rapid Prototyping ](https://www.sinbo-machining.com/services/rapid-prototyping/)[CNC Machining ](https://www.sinbo-machining.com/services/cnc-machining/)[Injection Molding Services ](https://www.sinbo-machining.com/services/injection-molding/)[Vacuum Casting ](https://www.sinbo-machining.com/services/vacuum-casting/)[Pressure Die Casting ](https://www.sinbo-machining.com/services/pressure-die-casting/)[Powder Metallurgy Services ](https://www.sinbo-machining.com/services/powder-metallurgy/)[Metal Injection Molding ](https://www.sinbo-machining.com/services/metal-injection-molding/)[Metal 3D Printing Services ](https://www.sinbo-machining.com/services/metal-3d-printing/)[Micro Molding Service ](https://www.sinbo-machining.com/services/micro-molding/)[About Us ](https://www.sinbo-machining.com/about/)[Resources ](https://www.sinbo-machining.com/resources/)[Case ](https://www.sinbo-machining.com/case/)[Blog ](https://www.sinbo-machining.com/blog/)[Contact ](https://www.sinbo-machining.com/contact/)
# Powder Metallurgy Manufacturing
Pressed and sintered metal parts with material, density, tolerance and finishing review ±0.025mm Dimensional Accuracy 500 ton Compaction Force 95-99% Density Control 20+ years PM Experience
## Precision Powder Metallurgy
Our powder metallurgy services offer cost-effective solutions for complex metal components with excellent material utilization and design flexibility. We specialize in high-volume production of precision parts with tight tolerances and superior mechanical properties. With advanced compaction technology and controlled atmosphere sintering, we produce components ranging from simple bushings to complex multi-level gears and structural parts for demanding applications. ISO 9001:2015 Certified IATF 16949:2016 Near Net Shape Material Optimization  [Powder metallurgy process]
## Powder Metallurgy Process
1
### Powder Mixing
Blending of metal powders with lubricants and additives for optimal flow and compaction 2
### Compaction
High-pressure forming of powder in precision tooling to achieve green density 3
### Sintering
Controlled atmosphere heat treatment for particle bonding and density development 4
### Finishing
Secondary operations including sizing, machining, and surface treatment
## Technical Capabilities

### Equipment Specifications
Press Capacity 5-500 tons Press Types Mechanical/Hydraulic Part Size Up to 200mm Part Weight 0.1g - 2kg Production Rate 10-120 ppm
### Material Systems

#### Ferrous
- Iron & Steel
- Stainless Steel
- Tool Steel
- Alloy Steel

#### Non-Ferrous
- Copper & Brass
- Bronze
- Aluminum
- Titanium

### Quality Standards
±0.025mm Dimensional Tolerance 95-99% Relative Density Cpk≥1.33 Process Capability 0.3% Defect Rate
## Industry Applications

### Automotive
Transmission gears, connecting rods, valve seats, pump components, bearings
### Industrial Machinery
Gear components, bearings, bushings, structural parts, cutting tools
### Consumer Goods
Appliance components, hardware, power tool parts, recreational equipment
## Ready to Start Your Powder Metallurgy Project?
Contact us today for a detailed quote and consultation [Get Instant Quote ](https://www.sinbo-machining.com/quote/)