# Titanium for CNC: Grade 2 vs Ti-6Al-4V Guide

> Practical titanium alloy guide: Grade 2 vs Ti-6Al-4V — when titanium is worth the cost, machining challenges, heat treatment, surface treatment, and common mistakes.

https://www.sinbo-machining.com/wiki/materials/titanium/

---

## On This Page

- Is Titanium Worth It?
- Grade 2 vs Ti-6Al-4V
- Machining Titanium — The Hard Truth
- Surface Treatment
- Common Mistakes
- Frequently Asked Questions

# Titanium Alloys
Titanium is impressive on paper — strong, light, corrosion-proof. It's also expensive, slow to machine, and often specified when aluminum or stainless would do the job at half the cost. This page helps you decide when titanium is genuinely needed and how to handle it. [Deep dive: Titanium vs Aluminum for Aerospace and Medical Parts: How to Choose ](https://www.sinbo-machining.com/blog/titanium-vs-aluminum/)
## Is Titanium Worth It?

|  Your Situation |  Use Titanium? |  Better Alternative
|  Aerospace / airframe structural |  Yes |  —
|  Medical implants (biocompatibility) |  Yes |  —
|  Marine (saltwater, no heat) |  Maybe |  316L stainless is cheaper for non-load parts
|  Chemical processing (corrosive) |  Maybe |  Hastelloy or super duplex may be better
|  High strength-to-weight (non-aero) |  Maybe |  7075-T6 aluminum is cheaper if non-corrosive
|  Just need lightweight + strong |  No |  7075 aluminum (same strength, 40% the cost)
|  Just need corrosion resistance |  No |  316 stainless (5–10x cheaper)
|  Prototype / low volume |  No |  Prototype in aluminum or steel first
Cost reality check Titanium raw material costs 5–10x more than aluminum, and 3–5x more than stainless. Machining costs 2–3x more than steel due to low cutting speeds and rapid tool wear. Only specify titanium when you have a genuine requirement for its unique combination of strength, weight, and corrosion resistance.
## Grade 2 vs Ti-6Al-4V

|  Property |  Grade 2 (CP) |  Ti-6Al-4V (Grade 5)
|  Type |  Commercially pure |  Alpha-beta alloy
|  Tensile (MPa) |  275–410 |  895–930
|  Yield (MPa) |  170–275 |  825–860
|  Density (g/cm³) |  4.51 |  4.43
|  Hardness |  200–275 HB |  33–36 HRC
|  Weldable |  Yes |  Difficult (requires protection)
|  Heat treatable |  No |  Yes (aging increases strength)
|  Machinability |  Better |  Hard on tools
|  Relative cost |  1.0x |  1.3–1.5x
|  Use for |  Chemical, marine, biomedical |  Aerospace, high-strength
Simple rule Need corrosion resistance (not high strength)? Use Grade 2. Need high strength + light weight? Use Ti-6Al-4V. That covers 95% of titanium applications.
## Machining Titanium — The Hard Truth

|  Rule |  Detail
|  Low cutting speed |  30–60 m/min for Grade 2, 20–45 m/min for Ti-6Al-4V. Going faster just burns the tool without cutting faster.
|  Flood coolant |  Mandatory. Titanium has poor thermal conductivity — heat stays at the cutting edge. Without flood coolant, tool life drops to minutes.
|  Sharp tools, replaced frequently |  Titanium work-hardens. A dull tool creates a hardened surface layer that kills the next tool too.
|  Low rake angle |  Use positive rake tools but with a sharper edge. TiAlN or diamond-coated end mills last 3–5x longer.
|  Thin chips |  Keep radial depth of cut small. Thick chips in titanium generate too much heat. Multiple shallow passes.
|  Fire risk |  Titanium chips can ignite. Never use cutting oil — use water-based coolant. Clean chips regularly.
Titanium fire Fine titanium chips can ignite, especially in dry machining. Titanium fires burn at 3000°C+ and cannot be extinguished with water (they burn hotter). This is rare but real. Use water-based flood coolant and keep the machine clean of chips.
## Surface Treatment

|  Treatment |  Purpose |  Notes
|  Anodize (Type II) |  Color, wear resistance |  Produces blue/purple/gold colors. Popular for medical and aerospace.
|  Grit blasting |  Surface preparation |  Creates matte finish. Required before many coating processes.
|  Polishing |  Mirror finish |  Possible but labor-intensive. Titanium polishes well.
|  PVD coating |  Wear resistance |  TiN, CrN on titanium for reduced friction. Used in medical implants.

## Common Mistakes

|  Mistake |  What happens |  Correct approach
|  Specifying titanium when aluminum suffices |  Paying 5–10x material cost for no benefit |  Do the calculation: strength/weight/corrosion requirement. Most parts don't need titanium.
|  High cutting speed |  Tool burns out in minutes, poor surface finish |  Keep below 60 m/min for Grade 2, 45 m/min for Ti-6Al-4V
|  Using cutting oil |  Fire risk with titanium chips |  Water-based coolant only
|  Not changing tools frequently enough |  Work-hardened surface kills subsequent tools |  Replace at first sign of wear
|  Grade 2 for high-strength parts |  Yield only 275 MPa — weaker than 6061-T6 |  High strength requires Ti-6Al-4V

## Frequently Asked Questions

#### When is titanium worth the cost, and when should I use aluminum instead?
Specify titanium only where its combination of strength, weight and corrosion resistance is genuinely required: aerospace or airframe structure, and medical implants. Otherwise the alternatives win on cost. 7075-T6 aluminum gives the same strength at 40% of the titanium cost, and 316 stainless is 5–10x cheaper when only corrosion resistance is needed. Titanium raw material costs 5–10x more than aluminum and 3–5x more than stainless, machining costs 2–3x more than steel, and a prototype belongs in aluminum or steel first.

#### Should I use Grade 2 or Ti-6Al-4V?
Decide on strength first, then check the environment. Grade 2 commercially pure titanium gives tensile 275–410 MPa, yield 170–275 MPa, density 4.51 g/cm³ and hardness 200–275 HB; it is weldable and kinder to tooling. Ti-6Al-4V gives tensile 895–930 MPa, yield 825–860 MPa, density 4.43 g/cm³ and 33–36 HRC, but welding it is difficult and it is hard on tools. Simple rule: corrosion resistance without high strength means Grade 2; high strength at low weight means Ti-6Al-4V.

#### Why do titanium parts need slow speeds and flood coolant?
Keep the speed low and keep coolant flooding. Grade 2 runs 30–60 m/min and Ti-6Al-4V runs 20–45 m/min; going faster burns the tool without cutting faster, so stay under 60 m/min and 45 m/min respectively. Flood coolant is mandatory because titanium has poor thermal conductivity — heat stays at the cutting edge and tool life drops to minutes without it. Use positive rake tools with a sharp edge, and TiAlN or diamond-coated end mills last 3–5x longer.

#### How do I avoid titanium chip fires and work-hardening problems?
Never use cutting oil. Fine titanium chips can ignite, especially in dry machining, and a titanium fire burns at 3000°C+ and cannot be extinguished with water because it burns hotter — so use water-based flood coolant and keep the machine clean of chips. On the work-hardening side, replace tools frequently: a dull tool leaves a hardened surface layer that kills the next tool as well. Keep radial depth of cut small and take multiple shallow passes, because thick chips generate too much heat.