# Sheet Metal Tolerance & Surface Finish: Stack, Coating and Flatness

> Sheet metal tolerance guide: which process controls which dimension, bend and hole limits, how coating changes dimensions, plus flatness and finish specs.

https://www.sinbo-machining.com/wiki/sheet-metal/tolerance-and-surface/

---

## On This Page

- Which Process Controls Which Dimension
- Building a Realistic Tolerance Stack
- How Coatings Move Dimensions
- Declaring Flatness So Both Sides Agree
- Surface Finish: What to Specify
- Datum Strategy for Sheet Metal Parts
- Common Mistakes
- Related Sheet Metal Pages
- Frequently Asked Questions

# Tolerance and Surface Finish
Sheet metal tolerance is not one number. Cutting, forming, welding and finishing each control different features to different limits, and those limits are not equally tight. This page sets out which process owns which dimension, what the limits actually are, and how coatings and material move your numbers after the part is made.
## Which Process Controls Which Dimension
When a dimension is out of tolerance, the first question is which operation created it. The answer determines whether the fix belongs in the drawing, the flat pattern, the fixture or a machining operation.
|  Feature |  Controlled By |  Achievable |  Main Limiters
|  Cut profile / outline |  Laser cutting |  ±0.05mm |  Thickness, cut length, heat input, machine calibration
|  Hole diameter |  Laser cutting |  ±0.05mm |  Kerf variation with thickness; small holes less accurate
|  Hole position |  Laser cutting + sheet flatness |  ±0.1mm |  Clamping distortion, thermal relaxation, residual stress release
|  Bend angle |  Press brake |  ±1° |  Material spring-back, tool condition, operator over-bend
|  Flange length |  Flat pattern calculation |  ±0.5mm |  K-factor assumption, bend deduction convention
|  Flatness after forming |  Bending sequence |  Per review |  Part stiffness, spring-back, fixturing during bending
|  Flatness after welding |  Weld sequence and restraint |  Per review |  Weld shrinkage, heat input, part stiffness
|  Sealing face flatness |  Final machining |  Machined to spec |  Requires a machining operation after forming or welding
Rule of thumb: if a tolerance is tighter than about ±0.1mm on a formed feature, forming will not deliver it reliably. The options are to machine it after forming, or to redesign the feature so forming error does not matter.
## Building a Realistic Tolerance Stack
A sheet metal part passes through several operations and each one adds variation. The finished part carries all of them. The most common contributors on a bent, finished panel:
|  Contributor |  Typical Contribution |  Reducible By
|  Material thickness variation |  ±5% of nominal on mill sheet |  Specifying a thickness tolerance class on the drawing
|  Cut profile position |  ±0.05mm |  Little — this is close to the process limit
|  Flat pattern calculation |  ±0.2 to 0.5mm per bend |  Stating the K-factor; simpler single-bend geometry
|  Spring-back variation |  ±0.5° to 1° per bend |  Material control, tighter incoming specification
|  Coating buildup |  +0.06 to 0.12mm per side |  Thinner film, or machining after finishing
|  Weld shrinkage |  0.3 to 1.5mm on a welded assembly |  Design stiffness, sequence, or machining the critical face
For a fit-critical feature, the sensible approach is to stop stacking at the operation that can actually control it: specify machining after forming or finishing, and dimension that feature from the machined surfaces rather than from the raw part.
## How Coatings Move Dimensions

|  Finish |  Typical Build per Side |  Dimensional Effect
|  Powder coating |  60–120 µm |  Adds material; also rounds sharp edges slightly
|  E-coating |  15–25 µm |  Minimal; the most dimensionally stable coating
|  Hot-dip galvanizing |  60–100 µm plus process allowance |  Largest effect; threads and close fits need allowance or masking
|  Anodizing (aluminium) |  5–25 µm |  Small but grows the part; dielectric, so it cannot be conductive
|  Passivation |  Negligible |  No dimensional effect; surface treatment only
|  Brushing / polishing |  Material removed |  Slightly reduces dimension; nominal is the finished size
Galvanizing is the usual surprise. Because the build-up is larger and varies with part geometry, galvanized fasteners and close fits need either a larger allowance or masking. Decide that on the drawing rather than at assembly.
## Declaring Flatness So Both Sides Agree
Flatness without a measurement condition is not a requirement — it is a disagreement waiting to happen. Three things must be stated: - Which faces — flatness of the whole part, or a named surface such as a gasket land.
- Over what length — flatness over 200mm and over 1000mm are very different requirements.
- Support condition — supported at two points, supported fully, or free. A thin panel measured unsupported will never meet a figure derived from a supported part.
Where flatness is functionally important — a sealing face, a gasket land, a heat-sink interface — the reliable route is to machine it after forming or welding. That adds an operation, and it is much cheaper to know at quotation than to discover on the first article.
## Surface Finish: What to Specify

|  Surface State |  Typical Ra |  How to Specify It
|  As-cut laser edge |  Ra 3–6 µm |  Standard; no callout needed unless a heat-tint band is unacceptable
|  Deburred / edge broken |  Ra 1–3 µm on the edge |  Standard on all edges
|  Ground or machined face |  Ra 0.8–1.6 µm |  State the face, the Ra value and any flatness requirement
|  Brushed stainless |  Ra 0.5–1.6 µm |  Specify grain direction and which side is cosmetic
|  Powder coated |  Not measured as Ra |  Specify colour standard, coverage and thickness range, plus which face is visible
|  Sealing face |  As-machined |  State flatness, Ra and whether any edge break is permitted on that face
Mark the cosmetic side. On any visible part, mark both views with the cosmetic face and, for brushed or grain-finished surfaces, the grain direction. Without it the finish can arrive on the wrong side and the part is scrap — not because the finish is wrong, but because it is on the wrong face.
## Datum Strategy for Sheet Metal Parts
Sheet metal parts are thin, flexible and often slightly warped after forming, which makes datum choice harder than it looks. A large flat machined face is not available on a folded panel, so the datum is usually an edge or a locating hole.
|  Situation |  Recommended Datum |  Reason
|  Flat panel, no forming |  Two wide faces, opposed, with an edge as secondary |  Standard; the faces are stable on a flat part
|  Bent panel |  A locating hole plus a flange edge |  The only repeatable features on a formed part
|  Feature must stay round after forming |  Machine it after forming and datum from machined features |  Forming error otherwise moves the datum
|  Welded assembly |  Locating holes on the flat panel plus machined faces |  Warpage makes a formed edge an unreliable datum

## Common Mistakes

|  # |  Mistake |  Consequence |  Correct Approach
|  1 |  Flatness specified with no measurement condition |  Endless dispute; both parties technically correct |  State faces, length and support condition.
|  2 |  Fit dimensions given before the coating is specified |  Part does not fit after finishing |  Specify the coating, then allow for build-up; or finish then machine.
|  3 |  Tight tolerance on a hole that gets bent |  Oval hole; the fastener no longer seats properly |  Move the operation after forming, or dimension generously.
|  4 |  Tolerance carried from thin to thick material unchanged |  Unachievable; parts rejected |  Widen the tolerance with thickness, or change material.
|  5 |  Relying on the general tolerance block for hole position |  Position error accepted that should have been controlled |  Call out hole position explicitly on features that matter.
|  6 |  Sealing face with a standard edge break applied |  The gasket will not seal |  Mark the sealing face and state no deburr, or a specified one.
|  7 |  Galvanized part with threaded holes not masked |  Threads no longer fit their fasteners |  Mask the threads, or oversize and re-tap after galvanizing.
|  8 |  Cosmetic face not marked |  Finish on the wrong side; part is scrap |  Mark both views, including grain direction.

## Related Sheet Metal Pages
- [Design for Sheet Metal ](https://www.sinbo-machining.com/wiki/sheet-metal/design-for-sheet-metal/)— the geometry rules behind these tolerances
- [Bend Radius and Bend Allowance ](https://www.sinbo-machining.com/wiki/sheet-metal/bend-radius-and-bend-allowance/)— flat pattern accuracy and spring-back
- [Welding Distortion Control ](https://www.sinbo-machining.com/wiki/sheet-metal/welding-distortion-control/)— flatness on welded assemblies
- [Material Selection ](https://www.sinbo-machining.com/wiki/sheet-metal/material-selection/)— spring-back and thickness tolerance by alloy
Have a tolerance that looks impossible? Send the drawing. We will tell you whether it is achievable as drawn, achievable with a machining operation, or achievable only with a design change — and what each option costs. [Request a Feasibility Check ](https://www.sinbo-machining.com/quote/)
## Frequently Asked Questions

#### What tolerance can I expect on a laser-cut sheet metal part?
Standard laser cut profile tolerance is plus or minus 0.05mm. Hole position is looser at plus or minus 0.1mm, because sheet distortion from clamping and heat moves the hole slightly. Bend angle is plus or minus 1 degree, and flange length plus or minus 0.5mm. Plus or minus 0.02mm on the profile is achievable on favourable geometry but is quoted case by case rather than advertised as standard.

#### How much does powder coating change my dimensions?
Typically 60 to 120 micrometres per side, so a nominal 1.5mm part becomes about 1.7mm after coating. On a sliding fit or a press fit that matters; on a clearance hole with an oversize tolerance it does not. Either specify the coating before the fit dimensions so the supplier can compensate, or machine the critical feature after finishing. Galvanizing adds considerably more because the zinc layer is much thicker.

#### How should I specify flatness on a sheet metal part?
State the measurement condition: which faces, over what length, and whether the part is supported or free. Without that, two parties can measure the same part and both be right. For a sealing or gasket face, specify flatness on that surface specifically rather than on the whole part, and discuss whether machining after welding or bending is required to achieve it.

#### What does edge break mean and do I need to specify it?
A small chamfer or radius, typically 0.3 to 0.5mm, applied to every sharp edge so nobody is cut during handling and the coating has something to key onto. It is applied as standard and included in the price, so you do not need to specify it. You do need to specify a different edge condition on a sealing face, a gasket land, a mating datum, or any edge an operator touches.

#### Does a hole stay round after bending?
It depends on where it is. A hole well away from any bend stays round. A hole close to a bend line distorts during forming because the material stretches and compresses as it bends. Keep the hole centre at least one thickness plus the bend radius from the bend line, and at least three times thickness if it genuinely has to stay round - or move the operation to after forming.

#### What surface finish should I specify for a cosmetic part?
As-cut laser edge is roughly Ra 3 to 6 micrometres with a faint heat-affected band. For a visible edge specify edge break plus grain direction. For a brushed or polished stainless surface specify the direction and the Ra value, and expect stainless to be more demanding than powder coating, where the specification is normally colour plus a coverage standard rather than a texture measurement.

#### Why does tolerance increase on thicker material?
Because more heat is involved. A thicker sheet takes longer to cut through, absorbs more energy, and leaves more residual stress, so it distorts more during the cut and more during bending. Spring-back also rises with thickness and yield strength. The practical consequence is that a tolerance which is comfortable at 1.5mm may need review at 6mm, and generally cannot simply be carried over.

#### Should I put a general tolerance block on my drawing?
Yes, for everything you have not called out. Use a linear and angular general tolerance such as ISO 2768-m, and then override the specific features that matter with tighter callouts. Avoid relying on the general block for hole position or flange length on a part that is bent - those are forming-dependent and deserve explicit callouts rather than inheriting a general tolerance.