Finishing Services

20+ Finishing Methods
1000×1000mm Part Size
Advanced Equipment
ISO 9001 Certified

Professional Surface Finishing Solutions

Surface finishing is a critical stage in the manufacturing process that significantly enhances product appearance, corrosion resistance, wear resistance, and functionality. Our comprehensive finishing services cover various post-processing needs for metal and plastic parts.

From simple deburring and polishing to complex anodizing and plating treatments, we have advanced equipment and experienced technical teams to ensure every part meets expected surface quality requirements.

Why Choose Our Finishing Services?

  • Wide range of finishing processes and materials
  • ISO 9001:2015 certified quality system
  • Fast turnaround time: 3-7 days
  • Expert team with 15+ years experience
Surface Finishing Workshop

Surface Finishing Processes

Comprehensive surface treatment solutions for various materials and applications

Anodizing

Electrochemical process that creates a protective oxide layer on aluminum and other metals, enhancing corrosion resistance and enabling color dyeing.

Thickness: 5-25μm
Colors: Various
Materials: Aluminum, Ti, Mg

Plating

Metal coating process that deposits a thin layer of metal onto the surface, providing enhanced corrosion resistance, conductivity, and aesthetic appeal.

Types: Zn, Ni, Cr, Au, Ag
Thickness: 2-50μm
Materials: Most Metals

Powder Coating

Dry finishing process that applies a free-flowing dry powder electrostatically and cures under heat, creating a hard, durable finish.

Thickness: 50-150μm
Colors: Unlimited
Materials: Metal, Plastic

Polishing

Abrasive process that smooths and shines surfaces to achieve mirror-like finishes, removing scratches and imperfections for enhanced aesthetics.

Roughness: Ra 0.1-0.8μm
Finish: Mirror
Materials: All Metals

Bead Blasting

Surface treatment that propels abrasive media at high velocity to clean, smooth, or texture surfaces, creating uniform matte finishes.

Media: Glass, Alumina, Steel
Finish: Matte
Materials: All Metals

Electropolishing

Electrochemical process that removes material from the surface, improving micro-finish, reducing surface roughness, and enhancing corrosion resistance.

Roughness: Ra 0.2-0.8μm
Removal: 10-50μm
Materials: Stainless Steel

Technical Specifications

Detailed capabilities and quality standards

Equipment Capabilities

Part Size 1000×1000mm
Coating Thickness 5-150μm
Temperature Control ±2°C
Surface Roughness Ra 0.1-3.2μm
Processing Capacity 5000+ parts/day

Quality Standards

ISO 9001:2015

Quality management system certification

Salt Spray Testing

Corrosion resistance verification

Thickness Measurement

Coating thickness verification

Visual Inspection

Surface quality assessment

Industries We Serve

Trusted by leading companies across various industries

Automotive

Engine components, chassis parts, decorative finishes

Medical

Surgical instruments, implants, medical devices

Electronics

Connectors, housings, heat sinks

Aerospace

Aircraft components, fasteners, structural parts

Frequently Asked Questions

Common questions about our finishing services

Start Your Finishing Project Today

Get in touch with our experts for professional consultation and competitive quotes