Zinc Die Casting Parts - High Precision
Zinc Die Casting Components Zinc Die Casting Surface Zinc Die Casting Quality Zinc Die Casting Precision

锌合金 Die Casting 零件

快速规格

工艺

Hot Chamber Die Casting

材料

Zamak 3, Zamak 5

公差

±0.03mm

交期

2-3 周

最小起订量

500 件

Max Weight

5kg

产品概述

Zinc 压铸 零件 at 新博精密 offer 出色 dimensional 精度 and 表面处理 through hot chamber 压铸 technology. 我们的zinc casting 工艺 injects molten 锌合金 into 精密 steel molds under high pressure, producing 零件 具有严格 公差s, 优异 surface quality, and 复杂 geometries that 是 ideal for 精密 应用. 锌合金's low melting point and 优异 fluidity enable the 生产 of thin-walled 零件 具有复杂 详情 and fine 特性.

我们的zinc 合金 portfolio includes Zamak 3 for general purpose 应用 具有优异 castability and mechanical properties, Zamak 5 for enhanced strength and hardness, ZA-8 for improved creep resistance, and ZA-12 for 高强度 应用. 每个合金 formulation 是 optimized for specific properties 包括tensile strength、hardness, impact resistance,和corrosion resistance. 我们的experienced team provides 专业 guidance on 合金 selection to ensure your 锌合金 die cast 零件 meet your exact requirements.

Every zinc die cast part undergoes meticulous 质量控制 包括dimensional inspection、visual examination,和机械测试 when required. 我们为immediate use in your products提供comprehensive secondary operations 包括CNC 加工、表面处理ing, plating,和assembly to provide complete, ready-to-use 组件. With our USA 仓库 and efficient logistics, you 能够 receive your 锌合金 die cast 零件 快速ly, ready。 Our engineering team provides design for 压铸 guidance to optimize your 零件 for manufacturability and cost efficiency.

技术规格

工艺 Hot Chamber Die Casting
材料 Zamak 3, Zamak 5, ZA-8, ZA-12, ZA-27
Part Weight 0.1g - 5kg
Wall Thickness 0.5mm - 5mm
公差 ±0.03mm (±0.001")
表面处理 Ra 0.8-1.6μm (as-cast), Ra 0.4-0.8μm (polished)
交期 2-3 weeks (tooling), 1 周 (production)
最小起订量 500 pieces (production), 5000 件 (economical)
Certifications ISO 9001, IATF 16949

材料选项

Zamak 3

General purpose 具有优异 castability

Zamak 5

Enhanced strength and hardness

ZA-8

Improved creep resistance and strength

ZA-12

高强度 and bearing properties

ZA-27

Maximum strength and wear resistance

定制 Alloys

Specialized 合金s for specific 应用

应用领域

汽车工业

Hardware 组件 and decorative 零件

电子产品

Connectors, housings, and EMI shielding

Hardware

Handles, knobs, and hardware 组件

Appliances

Appliance 组件 and fittings

Building

Door handles, locks, and architectural hardware

Toys

Toy 组件 and 精密 零件

制造能力

5kg

Max Part Weight

±0.03mm

精密 公差

2-3

周 交期

500+

Years Experience

质量保证

ISO 9001:2015 Certification

ISO 9001:2015

IATF 16949:2016 Certification

IATF 16949:2016

ISO 14001:2015 Certification

ISO 14001:2015

SA 8000:2014 Certification

SA 8000:2014

常见问题

What is the 最小起订量 quantity?

我们的最小起订量 quantity 是 500 pieces for 生产 runs. For 原型 quantities, we 能够 accommodate smaller orders 具有appropriate tooling costs. Economical 生产 typically begins at 5000 件 or more.

What is the typical 交期?

Tooling 交货期 是 typically 2-3 weeks depending on mold 复杂ity. 生产 交期 是 1 周 after tooling 是 complete. Expedited options 是 available for urgent requirements.

What file formats do you accept?

We accept STEP, IGES, Parasolid, and native CAD files. 我们的engineering team 能够 work 具有various formats and provide design for 压铸 guidance to optimize your 零件 for manufacturability.

What post-processing options are available?

我们为严格 公差s, shot blasting for surface preparation, plating (chrome, nickel, 锌合金), 粉末涂层, and assembly 服务 for complete 组件提供comprehensive post-工艺ing including CNC 加工。

What are the advantages of 锌合金 die casting?

锌合金 压铸 offers 优异 dimensional 精度, smooth 表面处理, 高强度-to-weight ratio, good corrosion resistance, 优异 electrical conductivity, and the ability to produce thin-walled 零件 具有复杂 geometries. 锌合金's low melting point also enables 快速er cycle times and longer tool life.

Can 锌合金 parts be plated?

Yes, zinc die cast 零件 能够 be plated 具有various finishes 包括chrome、nickel, 铜,和锌合金 plating. Plating enhances corrosion resistance, improves appearance, and provides additional surface properties for specific 应用.

Why Choose 新博精密

专业工程

20+ years of 锌合金 压铸 experience 具有专业 design guidance

快速 交付

2-3 周 tooling 交期 具有expedited options available

质量 Certified

ISO 9001, IATF 16949 认证 quality management systems

Dedicated 支持

Personal engineering support 来自design to 交付

Ready to Get Started?

Get an instant quote for your 锌合金 压铸 project today

相关产品

Aluminum Die Casting Services

铝合金 Die Casting

高精度 铝合金 零件

Learn More →
Magnesium Die Casting

镁合金 Die Casting

轻量化 镁合金 组件

Learn More →
Pressure Die Casting

Pressure Die Casting

High pressure casting 服务

Learn More →
Custom Die Casting Molds

定制 Molds

精密 压铸 tooling

Learn More →